Seven measures to reduce defects in mold processing

Release time:2021-08-23

In order to improve the performance of the mold, many manufacturers will process the mold properly. Mold processing refers to the processing of forming and punching tools. In addition, it also includes cutting die and die-cutting die. However, in many cases, the mold is processed. It will also reflect processing defects, resulting in the decline of mold performance. How to establish mold processing defects? The following seven measures can accumulate mold processing defects.


1. Reasonable selection and dressing of grinding wheel


White corundum grinding wheel is better. Its performance is hard and brittle, and it is easy to produce new cutting edges. Therefore, the cutting force is small and the grinding heat is small. Select medium particle size, such as 46 ~ 60 mesh. The hardness of the grinding wheel is medium soft and medium soft (ZR1, Zr2 and R1, R2), that is, coarse-grained, low hardness grinding wheel, good self excitation can reduce the cutting heat.


It is very important to choose a suitable grinding wheel for fine grinding. GD single crystal corundum grinding wheel is more suitable for high vanadium and high molybdenum conditions of die steel. When machining cemented carbide and materials with high quenching hardness, organic bond diamond is preferred. The self grinding performance of grinding wheel and organic bond grinding wheel is good, and the roughness of grinding workpiece can reach Ra0.2 μ m。 In recent years, with the application of new materials, CBN (cubic boron nitride) grinding wheels have shown good machining results. The effect of finish machining on CNC forming grinder, coordinate grinder and CNC Internal and external grinder is better than that of other types of grinding wheels.


In the grinding process, attention should be paid to timely dressing the grinding wheel to keep it sharp. After passivation, the grinding wheel will slip and squeeze on the surface of the workpiece, causing burns on the surface of the workpiece and reducing its strength.


2. Rational use of cooling lubricants


Play the three functions of cooling, flushing and lubrication, keep the cooling and lubrication clean, control the grinding heat within the allowable range, and prevent the thermal deformation of the workpiece. Improve the cooling conditions during grinding, such as using oil immersed grinding wheel or internally cooled grinding wheel. When the cutting fluid is introduced into the center of the grinding wheel, the cutting fluid can directly enter the grinding area, which has an effective cooling effect and prevents the workpiece surface from being burned.


3. Try to reduce the quenching stress after heat treatment


Due to the effect of quenching stress and grinding force, the phase transformation of network carbonized structure is easy to cause workpiece cracks. For high-precision dies, in order to eliminate grinding residual stress, low-temperature aging treatment should be carried out after grinding to improve toughness.


4. Eliminate grinding stress


The mold can also be immersed in a salt bath at 260 ~ 315 ℃ for 1.5 minutes, and then cooled in oil at 30 ℃, which can reduce the hardness by 1hrc and the residual stress by 40% - 65%.


5. Constant temperature grinding


For precision grinding of precision dies with dimensional tolerance within 0.01mm, attention should be paid to the influence of ambient temperature, and constant temperature grinding is required. The calculation shows that for a 300mm long steel, when the temperature difference is 3 ℃, the material will have 10.8 μ Change about M (10.8=1.2 × three × 3. The deformation per 100mm is 1.2 μ M/ ℃), and each finishing process needs to consider the influence of this factor.


6. Electrolytic grinding processing


Improve mold manufacturing accuracy and surface quality. During electrolytic grinding, the grinding wheel scrapes off the oxide film: instead of grinding metal, the grinding force is small, the grinding heat is small, and there will be no grinding burrs, cracks, burns, etc. the surface roughness can generally be better than ra0.16 μ m; In addition, the wear of grinding wheel is small, such as the grinding of cemented carbide. The wear amount of silicon carbide grinding wheel is about 400% - 600% of the weight of cemented carbide being ground. When electrolytic grinding is used, the wear of grinding wheel can only remove 50% - 100% of cemented carbide.


7. Reasonable selection of grinding amount


Fine grinding mode is adopted, with small radial feed and uniform fine grinding. If the radial feed rate and the speed of the grinding wheel are properly reduced and the axial feed rate is increased, the contact area between the grinding wheel and the workpiece can be reduced, the heat dissipation conditions can be improved and the temperature of the workpiece can be increased. The surface can be effectively controlled.

Copyright: Shenzhen Zhongyuan Plastic Co., Ltd. | mold processing customized manufacturer. If you want to know the processing price of the factory, how much is it, and which is good, please contact us Yue ICP Bei No. 17060480
国内精产熟女自线一二三区-六月丁香婷婷在线观看| 久久久噜噜噜久久狠狠50岁-精品一区二区三区av| 欧美三级韩国三级日本三斤-日本不卡一区不卡二区| 国产av一区二区三区日韩接吻-av网址在线播放网站| 成人免费资源在线观看-欧美国产日韩高清在线综合| av一区免费在线观看-中文字幕日韩国产精品视频| 国产精品一区二区在线免费-久久精品国产亚洲av热明星| 亚洲国产中文欧美一区二区三区-国产精品一区二区视频成人| 人妻互换精品一区二区-夜夜爽一区二区三区视频| 欧美日韩黑人在线播放-51在线精品免费视频观看| 日韩欧美国产综合久久-国产精品一起草在线观看| 久色高清精品在线国产-国产精品视频一区三区四区| 国产午夜精品理论片A级漫画-久久精品国产99亚洲精品| 欧美黄色三级视频网站-国产九九热视频在线观看| 黄色91av免费在线观看-欧美黄片一级在线观看| 亚洲av日韩五月天久热精品-国产日韩欧美一区二区三区群战| 深夜三级福利在线播放-日韩精品一区二区在线天天狠天| 国产剧情av中文字幕-五月婷婷在线手机视频| 亚洲永久免费在线观看-亚洲欧美导航一区二区导航| 国产人妻人伦精品日本-国产98超碰人人做人人爱| 日韩国产一区二区三区在线-精品日韩人妻少妇av| 91大神国内精品免费网站-亚洲免费电影一区二区| 国产精品一区二区欧美视频-国产一区二区三区天码| 日韩亚洲一区二区三区av-欧美综合在线观看一区二区三区| 亚洲一区二区免费av-中文字幕人妻久久久一区二区三区| 蜜臀av日日欢夜夜爽一区-av在线免费永久播放| 亚洲精品蜜桃在线观看-国产欧美日韩在线观看精品观看| 熟妇勾子乱一区二区三区-欧美爱爱视频一区二区| 欧美精品国产白浆久久正在-国产精彩视频一区二区三区| av一区免费在线观看-中文字幕日韩国产精品视频| 91大神国内精品免费网站-亚洲免费电影一区二区| 午夜精品午夜福利在线-内射无套内射国产精品视频| 亚洲最新国产无人区123-黄片一区二区在线观看| 国产剧情av中文字幕-五月婷婷在线手机视频| 亚洲欧美激情自拍色图-国产亚洲精品sese在线播放| 日本中文字幕啊啊啊啊-久久精品伊人久久精品伊人| 天天日天天干天天综合-99久久综合狠狠综合久久| 国产高清av免费在线观看-黄片毛片大全一区二区三区| 欧美日韩国产综合四区-爆操极品尤物熟妇14p| 欧美字幕一区二区三区-好吊妞欧美一区二区在线观看| 精品亚洲卡一卡2卡三卡乱码-一区三区二插女人高潮在线观看|